Welding Procedure
With gas metal-arc welding, the weld metal should be deposited in stringer beads, maintaining a small molten pool to avoid overheating the hot short silicon bronze base metal. Use argon gas for shielding and relatively high welding travel speeds.
With the gas-tungsten arc welding process, welding is accomplished with DCEN current and argon or helium gas shielding. ACHF with argon gas shielding may be used to take advantage of the arc cleaning action.
Preheat
Preheat slightly to remove moisture.
Interpass temperature should not exceed 150°F (66°C).
Chemistry | |
% (filler metal) | |
Copper | Balance |
Silicon | 2.8 – 4.0 |
Zinc | 1.0 max. |
Tin | 1.0 max. |
Manganese | 1.5 max. |
Iron | 0.50 max. |
Aluminum | 0.01 max. |
Lead | 0.02 max. |
Others | 0.50 max. |
Mechanical Properties | |
(Nominal all-weld metal values) | |
Tensile Strength ksi | 50 (350 MPa) |
Elongation, % in 2″ (51 mm) | 40 |
BHN (500 kg) 1/4″ deposit | 80 |
Specifications
AWS A5.7 Class ER CuSi-A
Document Download
SIL-TRODE® Technical Data Sheet